国产不卡福利一二三区_欧美精品日韩在线不卡蜜芽_在线观看欧美少妇高清_老熟妇乱子伦中文字幕_国产精品夜色视频_国产亚洲AV丝袜无码_欧美一区二区三区在观看线_影音先锋日本不卡资源_h视频网站免费无遮挡不卡_日韩丝袜老师无码AV

Valve Welding Inspection

Column:Technical service Time:2022-09-17
shared:
Valve welding inspection is generally divided into two parts:

Valve welding inspection is generally divided into two parts:


1. Document review


Need to provide WPS, PQR, welder qualification WPQ.


Whether the provided WPS covers the base metal, welding consumables, welding method, groove form, thickness, preheating, post-weld heat treatment and other important variables required by the order.


According to ASME Volume IX and WPS assessed by NB/T47014, there are corresponding important variable regulations. If important variables change, they must be reassessed.


2. On-site welding inspection


VT (visual inspection) is usually used to check for obvious welding defects such as cracks, undercuts, weld flashes, poor forming, burn through, spatter, etc.


For the surfacing of the sealing surface, PT is usually used to check whether there are cracks, and the hardness of the sealing surface needs to be checked;


Check the inlay welding between the valve seat and the valve body, basically as long as the appearance is flat, there is no undercut, dislocation and welding flash.


Inspection of structural welding such as extension pipes, RT or UT inspection of internal quality is required when required by the order.